Crystal growth process: | 3*3*0.3 CVD |
Color: | Optical grade- Colorless, |
Mechanic grade - Brownish | |
Advantage: | 1) Regular shape, uniform size. The size can be strictly controlled according to customer needs. 2) High repurchase rate and high cost performance, well received by customers. |
Orientation: | 4pt/100 |
2pt/110 | |
Shape: | Square |
Lateral Dimensions Measured | to smaller side |
Edges | Laser Cut |
Laser Kerf | < 3° |
Lateral Tolerance: | +0.1/-0 mm |
Roughness, Ra | Two sides polished, Ra < 30 nm |
Thickness Tolerance | +/- 0.05 mm |
Boron Concentration [B]: | <0.05 ppm |
Nitrogen Concentration: | Optical grade <10ppm |
Mechanical grade - <50 ppm |